Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
IDI Composites 46-16 Thermoset Polyester, Molding Premium high strength electrical grade with excellent resistance to smoke generation, weathering, and corrosive environments.Data provided by the manufacturer. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
IDI Composites C-105 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C25 S006 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.80 - 1.82 g/cc | 0.0650 - 0.0658 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF) Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3.. |
|||
Density | 1.80 g/cc @Temperature 25.0 °C |
0.0650 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 32245 Phenolic, Injection Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | Cured |
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-63 Compression Molded PPS Compound, 50% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-69 Compression Molded PPS Compound, 35% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
Epoxyset Epoxibond EB-315 Low Expansion Epoxy Adhesive EB-315 is a highly filled, heat curing, high temperature resistant epoxy adhesive. Due to its low coefficient of thermal expansion and outgassing, it can be used for bonding and sealing in critical .. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
Polyram RamOfin PPC350M6 Polypropylene, 30% Mineral Filled 30% Mineral filled, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Density | 1.80 g/cc | 0.0650 lb/in³ | |
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther.. |