Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
PolyOne OnForce™ LFT NN-60LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Substrate Property; Arlon SQA-TMS-024 |
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate
(discontinue Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPET® KP133G45 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM F1315 |
Thermoseal ML-5270 PTG Gasketing Thermoseal ML-5270 is a high performance synthetic fiber and polychloroprene binder gasket material that is resistant to refrigerants and oil mixtures. Its unique Multi-Layer Technology structure pr.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Westlake Plastics Tefzel® 2181 ETFE Products made from Tefzel® HT-2181 resin are suitable for a variety of processes and demanding end uses. They are mechanically tough and offer an excellent balance of properties. These products p.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Zircar Refractory Composites RS-A3 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Cytec Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 545 BK504 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness excellent dimensional stability and cr.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Cured |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 Method A |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.70 - 1.80 g/cc | 0.0614 - 0.0650 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Density | 1.70 - 1.75 g/cc | 0.0614 - 0.0632 lb/in³ | |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |