Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.56 - 1.60 g/cc | 0.0564 - 0.0578 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 425 Rigid PVC, Extrusion Electric channels |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | |
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer LNP THERMOCOMP* KF004A is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East) LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ASTM D792 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183-87 |
Wellman Wellamid® FRGF1850-BK1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | Layer 2, Silicone Property; Arlon SQA-TMS-024 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Density | 1.56 g/cc @Temperature 23.0 °C |
0.0564 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® K223-HMS6 Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
DSM Arnite® TV4 230 PBT-15% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |