Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | wet density (as supplied) |
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
LATI Latilub 80-10T K/15 PPS, 15% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO R 1183 |
Schwartz Technical Plastics MITELA® HD8B Cotton Fabric, Special Quality Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 (Asia Pacific) LNP* LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing PTFE, Glass Fiber, Silicone. Added features of this material include: Internally Lubricated. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, In.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated 20% Glass Reinforced, PTFE Lubricated |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Plenco 7591 Phenolic, Briquette, Injection Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
Loctite® Ultra Grey® 5999 Flange Sealant Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry) Description: Ultramid 66 H2 G/35-V0KB NAT0046 is a 35% glass reinforced, heat stabilized injection molding grade. It is a V-0 self-extinguishing grade, with phosphorous. It offers good flowability a.. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
BASF Paliogen® Red L 3880 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
BASF Paliogen® Red L 3910 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
Loctite® Ultra Grey® 5699 Flange Sealant Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Density | 1.45 g/cc | 0.0524 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty.. |