Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0466 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
STN EN ISO 1183-1
Plastcom SLOVAMID 6 GB 30 HI PA6 reinforced with glass beads, improved impact strength
PA 6 for injection molding, reinforced with 30% glass beads, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber
Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC (Europe-Africa-Middle East)
LNP* Lubricomp* DL0029E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Flame Retardant.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Polycasa COPOL PETG
QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Density 1.29 g/cc
0.0466 lb/in³
LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DE0039 PC
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10
LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive)
CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provid..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding
Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance..
Density 1.29 g/cc
0.0466 lb/in³
DAM; ISO 1183
DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Addiplast Addinyl B2 V20 Nylon 6. 20% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry)
Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Azoty Tarnow™ TARNOFORM 300 CI4 POM
Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Addiplast Addinyl C2 V20 Nylon 66/6, 20% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds PM 5840 Flexible PVC, Extrusion
Gaskets for frames
Density 1.29 g/cc
0.0466 lb/in³
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved