Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 M2 Nylon 6.6 for injection molding, 2% molybdenum disulphide lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Density | 1.15 - 1.61 g/cc | 0.0415 - 0.0582 lb/in³ | Average value: 1.42 g/cc Grade Count:27 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade
(discontinued **) OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
DuPont™ Dartek® B-601 Nylon 6,6 Barrier Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A strong transparent nylon type 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. Can be pri.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Huntsman IROGRAN® CA116-201 TPU-Polyester Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Global PC/ABS-1211 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 5801 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO R 1183 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Solvay SIPOMER® WAM Allyl / Ureido Monomer Description: Specialty monomer for Wet Adhesion PromotionIdentification: ALLYL / UREIDO MONOMERCAS: 90412 – 00 – 3EINECS: 291 – 480 – 2Solubility: Soluble in water. Insoluble in .. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Chase Plastics CP Pryme® NN100M2HS (Dry) Nylon 66, Lubricated, Heat Stabilized Features: Good chemical resistanceFast cycleDurableHeat stabilizedLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Wanhua Chemical Wanthane® WHT-8280H Super Hard Polyether-Based TPU Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | Compound; ASTM D792 |
Borealis Casico™ FR4802 Non-Halogen Flame Retardant Insulation/Jacketing Compound Borstar FR4802 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4802 offers a unique combination of good extrusion p.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Covestro Apec® HT KU 1-9354/1 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Covestro Bayblend® T 84 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Covestro Desmopan® 588 Thermoplastic Polyurethane Desmopan 588 is a TPU on the basis of a special ether with good microbe-resistance.Applications: Cable sheathing, hoses, profiles.Information provided by Bayer.As of 1 September 2015, Bayer Material.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
DSM Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components wh.. |
|||
Density | 1.15 - 1.45 g/cc | 0.0415 - 0.0524 lb/in³ | Average value: 1.27 g/cc Grade Count:18 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |