Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
M. Holland Company IS350 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Structural Foam, Household Goods, Housings, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | |
Ineos ABS Lustran® QE 1045 A, Injection Grade
(discontinued **) Injection molding grade, high modulus, only available in black.Applications: For automotive application.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | (DAM) |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL HN731SE PPE+HIPS (Europe-Africa-Middle East) PPE+PS blend. For medical devices and pharmaceutical applications. NORYL HN731SE is an unfilled material, with a Vicat B/120 of 135C according ISO 306. Healthcare management of change, biocompati.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
Covestro Desmopan® DP 9370A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® 2D 20 nat PA612 Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | |
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend Grade with high resistance to heat deformation and outstanding impact strength. For auto parts such as air vents or the instrument panel; also used for door-mirror housings.Data was collected by IS.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
BASF Ultramid® BU50I BK 106 PA6 (Conditioned) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® P270WO PPO An extrusion grade for high temperature applications requiring flame retardancy as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | Uncured |
3M Scotch-Weld™ EC100 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | |
Arkema Group Orgalloy® LE 6006 Nylon Alloy, 6% Glass Fiber Reinforced (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).6% glass fiber reinforced. Medium stiffness, good thermomechanical.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | Uncured |
3M Scotch-Weld™ SF100 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, High Flow Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |
|||
Density | 1.06 g/cc | 0.0383 lb/in³ | |
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers |