Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc | 0.0379 lb/in³ | Load Density; ASTM D792 |
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular .. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Network Polymers NPP 30-1200 TF20 Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Pasargad Polymer Peyvand Pasalen 3P-H3120B Polypropylene, 20% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Density | 1.05 - 1.48 g/cc | 0.0379 - 0.0535 lb/in³ | Average value: 1.13 g/cc Grade Count:123 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Density | 1.05 - 1.29 g/cc | 0.0379 - 0.0466 lb/in³ | Average value: 1.14 g/cc Grade Count:29 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792B |
LyondellBasell Astryn 65F4-2 Polypropylene Homopolymer, 20% Talc Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, excellent impact and stiffness balance, good dimensional stability, excellent heat resistance, good colo.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styrolution Novodur® HH-106 ABS Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792; ISO 1183/B |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN®-V 400T ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |