Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Reliance Industries METABOLIX PHO Information provided by Reliance Industries |
|||
Density | 1.02 g/cc @Thickness 3.17 mm |
0.0368 lb/in³ @Thickness 0.125 in |
injection molded specimen; ISO 1183 |
Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued .. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay ALKAMULS® 696 D Surfactant Description: Ethoxylated castor oil of HLB close to 8, useful as an emulsifier in liquid formulationsIdentification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Available in: Asia Pacific, Eu.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay ALKAMULS® 696 Surfactant Description: Ethoxylated castor oil of HLB close to 8, useful as an emulsifier in liquid formulationsIdentification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Available in: Asia Pacific, E.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay ALKAMULS® R 81 Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 9.Chemical Name: ETHOXYLATED CASTOR OILCAS: 61791 - 12 – 6Solubil.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Polyplastics TOPAS® 8007 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Water adsorption is small and barrier properties are good, making this grade particularly suitable for package applications for products that dislike moisture. Grade 8007 has lower coefficient of el.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Density | 1.02 g/cc @Temperature 290 °C |
0.0368 lb/in³ @Temperature 554 °F |
Melt |
Covestro Makrolon® 1837* Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable.. |
|||
Density | 1.02 g/cc @Temperature 300 °C |
0.0368 lb/in³ @Temperature 572 °F |
Melt |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Density | 1.02 g/cc @Temperature 280 °C |
0.0368 lb/in³ @Temperature 536 °F |
Melt |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
Density | 1.02 g/cc @Temperature 290 °C |
0.0368 lb/in³ @Temperature 554 °F |
Melt |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Density | 1.02 g/cc @Temperature 280 °C |
0.0368 lb/in³ @Temperature 536 °F |
Melt |
Covestro Makrolon® Rx2430 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183/A |
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e.. |
|||
Density | 1.02 g/cc @Temperature 280 °C |
0.0368 lb/in³ @Temperature 536 °F |
Melt |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO R1183 |
Arkema Group Orgalloy® LE 60 LM Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | Mixed; ASTM D891 |
3M Scotchcast™ 2136 Potting Kit The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat.. |
|||
Density | 1.02 - 1.06 g/cc | 0.0368 - 0.0383 lb/in³ | Spec; ISO 1183-1 |
Axion Polymers Axpoly® PS13 1011 High Impact Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
BASF Styroclear GH 58 SBC Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 426 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr.. |
|||
Density | 1.02 - 1.07 g/cc | 0.0368 - 0.0387 lb/in³ | Part B |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay RHODISOLV® GREEN 21 Solvent Identification: BLEND OF SOLVENTSAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Insoluble in water. Soluble in most polar and aromatic solvents. Applications: Solvent.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | |
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |