BASF Styroclear GH 58 SBC

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer BASF
Trade Name Styroclear
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Styroclear GH 58 SBC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance for general molding applications. Styroclear GH 58 may be suitable for conventional thermoplastics processing technologies such as injection molding.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption 0.070 %
0.070 %
ISO 62
Melt Flow 16 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM Test
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM Test
Tensile Strength, Yield 28.0 MPa
4060 psi
2 in/min; ASTM Test
Elongation at Break 43 %
43 %
2 in/min; ASTM Test
Tensile Modulus 1.68 GPa
244 ksi
2 in/min; ASTM Test
Flexural Strength 33.0 MPa
4790 psi
ASTM Test
Flexural Modulus 1.50 GPa
218 ksi
ASTM Test
Dart Drop, Total Energy 0.600 J
0.443 ft-lb
ASTM Test
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM Test
Vicat Softening Point 90.0 °C
194 °F
Rate "B" Loading 1 (120 degC/h 10N); ASTM Test
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Electrical Properties Metric English Comments
Dissipation Factor 0.00030

@Frequency 1e+9 Hz
0.00030

@Frequency 1e+9 Hz
ASTM Data
0.00080

@Frequency 1.00e+6 Hz
0.00080

@Frequency 1.00e+6 Hz
ASTM Data
Processing Properties Metric English Comments
Melt Temperature 180 - 235 °C
356 - 455 °F
Injection Molding
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Molding
Descriptive Properties Value Comments
Color Clear
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding