Polymer Property : Density = 0.0346 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
Network Polymers NPP 50-0158
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin
Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin  (discontinued **)
Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th..
Density 0.957 g/cc
0.0346 lb/in³
ASTM D1505
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE  (discontinued **)
General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a..
Density 0.959 g/cc
0.0346 lb/in³
ASTM D 792
Total Finathene® 7208 HDPE extrusion resin  (discontinued **)
Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics ..
Density 0.958 g/cc
0.0346 lb/in³
ASTM D 792
Total Finathene® 3407B Black HDPE pipe grade  (discontinued **)
Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To..
Density 0.957 g/cc
0.0346 lb/in³
Exxon Method
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature ..
Density 0.959 g/cc
0.0346 lb/in³
ASTM D1475
Humiseal 1C65 Silicone Conformal Coating
Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..
Density 0.959 - 0.983 g/cc
0.0346 - 0.0355 lb/in³
Lord Adhesives Flocklok® Catalyst 1
Flocklok Catalyst 1 will accelerate the cure rate of Flocklok adhesives and will not diminish the work life, unless exposed to moisture. There is minimal impact on VOC levels, as low levels of the c..
Density 0.959 g/cc

@Temperature 20.0 °C
0.0346 lb/in³

@Temperature 68.0 °F
LyondellBasell PMA Propylene glycol methyl ether acetate
Available in electronic grade.Information provided by Lyondell.
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
Iran Petrochemical (PCC) 60507 High Density Polyethylene
60507 is a HDPE injection molding grade which combines good flowability with balanced physical properties. This resin is well suited for general purpose applications requiring high stiffness. Applic..
Density 0.957 g/cc
0.0346 lb/in³
ISO 1183
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Density 0.957 g/cc
0.0346 lb/in³
ISO 1183
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene
I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance...
Density 0.959 g/cc
0.0346 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Density 0.957 g/cc
0.0346 lb/in³
ISO 1872/1
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding
Applications:Large dustbins and pailsPallet boxesFish cratesTechnical moldingInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Density 0.957 g/cc
0.0346 lb/in³
ISO 1183
Borealis BL2571 High Density Polyethylene
BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers..
Density 0.958 g/cc
0.0346 lb/in³
ISO 1183/ISO 1872-2
Borealis VL4580 High Density Polyethylene
VL4580 is a high density polyethylene. This grade is especially designed for monofilament production. Applications: ropes, twines, nets, straps and brushes.Information provided by Borealis AG
Density 0.959 g/cc
0.0346 lb/in³
ISO 1183
Total Xsene® BM 593 HDPE, blow molding
FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been es..
Density 0.957 g/cc
0.0346 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 02133EN2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 02133EN12 is a copolymer of ethylene and vinyl acetateAvailability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoFree Flowing Agent:..
Density 0.958 g/cc
0.0346 lb/in³
ExxonMobil method
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc..
Density 0.957 g/cc
0.0346 lb/in³
ASTM D4883
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin
Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme..
Density 0.958 - 0.964 g/cc
0.0346 - 0.0348 lb/in³
BRCP 4843
ExxonMobil Jayflex™ L911P Plasticizer
Appearance: Clear and FreeAvailability: North AmericaCAS Number: 685151-43-5Information provided by ExxonMobil
Density 0.959 g/cc
0.0346 lb/in³
Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin
CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan..
Density 0.957 g/cc
0.0346 lb/in³
ASTM-D792
Braskem GM5240PR HDPE High Density Extrusion Polyethylene
GM5240PR is a high-density polyethylene compound specially developed for the manufacturing of pipes, underground conduits, and steel pipe coating. This resin is produced with bimodal technology and ..
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu..
Density 0.958 g/cc
0.0346 lb/in³
ASTM D4883
ExxonMobil Paxon™ EA60-007 Blow Molding Resin  (discontinued **)
EA60-007 is an unstabilized blow molding grade high density polyethylene copolymer. The base resin can be compounded to incorporate such things as stabilizers, fillers, and colorants before process..
Density 0.958 g/cc
0.0346 lb/in³
Exxon Method
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom..
Density 0.958 g/cc
0.0346 lb/in³
ISO 1183
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Bormed HE2581-PH is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). Bormed HE2581-PH can as well be ..