ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
Mixed
Viscosity 10000 - 20000 cP
10000 - 20000 cP
B
115000 - 130000 cP
115000 - 130000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 - 20.7 MPa
2500 - 3000 psi
Elongation at Break 140 - 160 %
140 - 160 %
Tensile Modulus 0.276 - 0.345 GPa
40.0 - 50.0 ksi
Shear Strength 8.62 - 10.3 MPa
1250 - 1500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 40 - 45 min
40 - 45 min
Descriptive Properties Value Comments
Color Blue or white
Fixture Time 110-120 minutes
Gap Filling Max 1 in
Mix Ratio 10:1
By volume