Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.940 - 1.30 g/cc @Temperature 170 - 240 °C |
0.0340 - 0.0470 lb/in³ @Temperature 338 - 464 °F |
Average value: 1.04 g/cc Grade Count:27 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 155-1326 LMDPE Rotational Molding Resin Description: ICORENE 155-1326 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 2781 |
KKPC KOSYN KTR 301 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792-91 |
Micropol Microcene MC122 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP LNP* THERMOCOMP* MF001AS is a compound based on Polypropylene resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ISO 1183 |
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake Elevate™ EM518 18.5% Ethylene Vinyl Acetate Copolymer Westlake Elevate™ EM518 resin is an 18.5% EVA copolymer designed for injection molding, compounding, and foam. It has excellent low temperature brittleness properties, melt strength, and flexibilit.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM-D1505 |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183 |
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183/A |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | |
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema. |
|||
Density | 0.941 g/cc @Temperature 0.000 °C |
0.0340 lb/in³ @Temperature 32.0 °F |
|
BorsodChem ONGRONOX EHP 75 D peroxide-type initiator Chemical name: Bis-(2-ethylhexyl)-peroxi-dicarbonate.Mol. wt: 346.5g/mol.Active oxygen content: 4.62 %.Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 2-ethyl-hexan.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® VL 20 N HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Surlyn® 1825 Zinc Ionomer Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 2781 |
KKPC KOSYN KTR 402 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |