Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Borealis
Trade Name BorPEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible crosslinkable pipes. BorPEX HE 2515 is designed for the requirements in DIN 16892/BIN 16887 for hot water pressure pipes, e.g. floor heating, radiator connections and for domestic hot and cold water supply. Documentation is available on request.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ISO 1183
Melt Flow 1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
At 50 mm/min; ISO/DIS 6259
Tensile Strength, Yield 27.00 MPa
3916 psi
At 50 mm/min; ISO/DIS 6259
Elongation at Break 195 %
195 %
ISO/DIS 6259
Elongation at Yield 11 %
11 %
ISO/DIS 6259
Modulus of Elasticity 0.960 GPa
139 ksi
ISO 527
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
500 µm/m-°C

@Temperature 100 °C
278 µin/in-°F

@Temperature 212 °F
ASTM D696
Specific Heat Capacity 2.10 J/g-°C
0.502 BTU/lb-°F
Vicat Softening Point 126 °C
259 °F
ISO 306
Users viewing this material also viewed the following: