Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.992 - 1.44 g/cc | 0.0358 - 0.0520 lb/in³ | Average value: 1.21 g/cc Grade Count:211 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Density | 1.06 - 1.44 g/cc | 0.0383 - 0.0520 lb/in³ | Average value: 1.19 g/cc Grade Count:40 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Density | 1.10 - 1.44 g/cc | 0.0397 - 0.0520 lb/in³ | Average value: 1.21 g/cc Grade Count:81 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Density | 1.04 - 1.44 g/cc | 0.0375 - 0.0520 lb/in³ | Average value: 1.24 g/cc Grade Count:15 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.25 - 1.44 g/cc | 0.0452 - 0.0520 lb/in³ | Average value: 1.29 g/cc Grade Count:5 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Density | 1.21 - 1.44 g/cc | 0.0437 - 0.0520 lb/in³ | Average value: 1.32 g/cc Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 528/H Rigid PVC, Antishock Injection Molding Road drains |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 311 Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 63/K Flexible PVC, Sheathing General purpose, opaque surface |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 71 Flexible PVC, Sheathing General purposes |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 7550 Flexible PVC, Sheathing Coaxial sheaths |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 90/1 Flexible PVC, Insulation Lead Free Oil resistant insulation |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 88/1 Flexible PVC, Insulation Power cables |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 74 Flexible PVC, Flame Retardant Sheathing Mineral oil resistent |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 88 Flexible PVC, Flame Retardant Sheathing Operating temperature 105°C |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 509/1 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds HG 81 Flexible PVC, Sheathing for High Temperatures Operating temperature 105°C |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 81 Flexible PVC, Sheathing for High Temperatures Lead Free Sheath high flexibility |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 83 Flexible PVC, Sheathing for High Temperatures Lead Free Operating temperature 90°C |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 80/3 Flexible PVC, Sheathing Lead Free Sheath Oil resistance (90°C) |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 70/R Flexible PVC, Flame Retardant Sheathing Operating temperature 75°C |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 83 Flexible PVC, Extrusion Modified with Rubber Tubes for hot water |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 8350 Flexible PVC, Lead Free Sheath according to normal fiat type 70 9.91220 All. 28 |
|||
Density | 1.37 - 1.44 g/cc | 0.0495 - 0.0520 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 63/K Flexible PVC, Sheathing Lead Free Opaque sheath |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 92 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 90°C |
|||
Density | 0.650 - 1.44 g/cc | 0.0235 - 0.0520 lb/in³ | Average value: 1.20 g/cc Grade Count:332 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.960 - 1.44 g/cc | 0.0347 - 0.0520 lb/in³ | Average value: 1.12 g/cc Grade Count:37 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Density | 1.42 - 1.44 g/cc | 0.0513 - 0.0520 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT2100 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 84 Flexible PVC, Flame Retardant Sheathing Mineral oil resistant sheathing (80°C) |