Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | Average value: 1.15 g/cc Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Density | 0.900 - 1.15 g/cc | 0.0325 - 0.0415 lb/in³ | Average value: 1.06 g/cc Grade Count:60 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | Average value: 1.14 g/cc Grade Count:8 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0415 lb/in³ | Average value: 1.11 g/cc Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | ASTM D792 |
Global Atron 6601-B General Purpose Nylon 66 Information provided by Global Polymers Corporation. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.10 - 1.15 g/cc | 0.0397 - 0.0415 lb/in³ | |
Solvay MACKAM® MEJ Surfactant Product Description: Mackam MEJ is an amphoteric wetting agent produced from caprylic imidazoline. It is stable in high alkaline systems, compatible with phosphate builders and provides low, stable .. |
|||
Density | 1.00 - 1.15 g/cc | 0.0361 - 0.0415 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | Dry Density |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Density | 1.13 - 1.15 g/cc | 0.0408 - 0.0415 lb/in³ | Dry Density |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) at 50% RH Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0416 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6) Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0416 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6) Tecast® 6PAM is a molybdenum disulfide-filled cast nylon 6 used for general bearings and wear applications and for its superior strength and hardness.General Tecast® Cast Nylon Information: Tecast.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0415 lb/in³ | ASTM D792 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0415 lb/in³ | ASTM D792 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® A24 E 01 PA66 Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® A27 E PA66 Description: Ultramid® A27 E is a polyamide 66 grade for compounding.Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B40 L PA6 Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round .. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B40 LN PA6 Description: Ultramid® B40 LN is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film. Clarity and thermoformability are enhanced by the incorporation.. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B40 PA6 Description: Ultramid® B40 is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round pellets.Infor.. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | |
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | |
BASF Ultramid® B32 0.015 BOPA Film Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B33 L PA6 Description: Ultramid® B33 L is a lubricated polyamide 6 grade of intermediate viscosity that is well suited for the production of biaxial oriented and cast film and monofilaments. Product comes .. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B33 LV PA6 Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | |
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll Product comes in 2-2.5 mm round pellets.Information provided by BASF |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B36 PA6 Description: Ultramid® B36 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film and monofilaments. Product comes in 2-2.5 mm round .. |
|||
Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
BASF Ultramid® B36 LN 01 PA6 Description: Ultramid® B36 LN 01 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film. Clarity and thermoformability are enhanced b.. |