| Category | Polymer , Film , Thermoplastic , Nylon |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Ultramid® B32 0.015 BOPA Film.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | |
| Water Vapor Transmission | 43.0 g/m²/day | 2.77 g/100 in²/day | 85% RH |
| Oxygen Transmission Rate | 14.0 cc/m²/day | 0.902 cc/100 in²/day | 50% RH |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 250 MPa | 36300 psi | MD |
| 260 MPa | 37700 psi | TD | |
| Elongation at Break | 85 % | 85 % | TD |
| 90 % | 90 % | MD | |
| Tensile Modulus | 0.260 GPa | 37.7 ksi | MD |
| 3.00 GPa | 435 ksi | TD |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Commercial Status | Europe |