Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Ferro EG 2410 Specialty Glass Glass Type: Si-MG-Al Typical Powder Form: MVG Typical Application: Sintering Aid / Glaze Ferro offers a wide range of compositions for specialty applications including sintering aids used in the gl.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Indium Corp. Indalloy 192 Pure Aluminum Information Provided by Indium Corporation |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent |
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
LATI Latimass 63-06 D025 PA66 Specific density compound based on Polyamide 66 (PA66). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Schott S8802 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific) LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Density | 2.70 - 2.90 g/cc | 0.0975 - 0.105 lb/in³ | |
Tritex TREO Needled Blanket Insulation Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | Cured |
Chesterton ARC MX1 Vertical Build Extreme Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”).. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | Cured |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-10 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | Alloy 1100 Property (Annealed) |
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | AA 5005 |
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
ALIMEX 6082 T651 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |
|||
Density | 2.70 g/cc | 0.0975 lb/in³ | |
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |