| Category | Ceramic , Oxide , Aluminum Oxide , Silicon Oxide | 
| Manufacturer | Gouda Vuurvast | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Gouda Vuurvast AK 80 FM Dense Refractory Brick.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent | 
| Porosity | 17 % | 17 % | Apparent | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Thermal Conductivity |           1.90           W/m-K           @Temperature 650 °C  | 
                  13.2           BTU-in/hr-ft²-°F           @Temperature 1200 °F  | 
        |
|           2.10           W/m-K           @Temperature 100 °C  | 
                  14.6           BTU-in/hr-ft²-°F           @Temperature 212 °F  | 
        ||
|           2.20           W/m-K           @Temperature 1100 °C  | 
                  15.3           BTU-in/hr-ft²-°F           @Temperature 2010 °F  | 
        ||
| Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> | 
| 1700 °C | 3090 °F | 
| Component Elements Properties | Metric | English | Comments | 
|---|---|---|---|
| Al2O3 | 76 % | 76 % | |
| Fe2O3 | 0.30 % | 0.30 % | |
| SiO2 | 23 % | 23 % | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Segercone | 39 | |
| Thermal Shock Resistance | 30 cycles | DIN 51068 |