Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.30 g/cc | 0.0831 lb/in³ | Green |
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.30 g/cc @Temperature 20.0 °C |
0.0831 lb/in³ @Temperature 68.0 °F |
liquid |
Oceanchem Group Zinc Bromide Molecular Formula: ZnBr2Cas No.: 7699-45-8Mainly applied in ocean oil wells as complete liquid, stationary liquid and amend liquid.Information Provided by Oceanchem Group |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183-1 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | 2.3 g/cc Average. Minimum bulk density is 2.277 g/cc. |
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 599.063 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC50 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC8 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183 |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 Method A |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 Method A |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
BASF Paliotan® Yellow L 1240 Color Additive Description: Economical lead free pigment with good hiding, high chroma and color strengthSuitable for: Baking systems |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec GRADE A LAVA Machinable Ceramic GRADE A LAVA is a machineable ceramic that exhibits good electrical and heat resistance. It is excellent in applications where close tolerances must be held. This material is available in a variety .. |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | Apparent |
Gouda Vuurvast AK 45 Dense Refractory Brick Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av.. |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 584.054 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |