For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-direction CTELarge Panel Sizes AvailableLow Thermal Coefficient of ErBenefits:Higher Antenna EfficienciesLow Insertion LossMultiple boards per panel (reduced edge trim waste)Large antenna formatsTypical Applications:Base Station Antenna ApplicationsGPS and RFID Reader AntennasDigital Audio Broadcasting (DAB) Antennas (Satellite Radio)Electronic Surveillance, SIGINT and other RF applicationsInformation provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
ASTM D792 Method A
Water Absorption 0.040 %
0.040 %
IPC TM-650 2.6.2.2
Mechanical Properties Metric English Comments
Tensile Strength >= 138 MPa
>= 20000 psi
IPC TM-650 2.4.18
Modulus of Elasticity >= 4.83 GPa
>= 700 ksi
ASTM D638
Flexural Modulus >= 3.72 GPa
>= 540 ksi
ASTM D790
Compressive Modulus >= 2.41 GPa
>= 350 ksi
ASTM D695
Peel Strength 2.98 kN/m
17.0 pli
To Copper (1 oz.); A, TS; IPC TM-650 2.4.8
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 0.000 - 100 °C
8.89 µin/in-°F

@Temperature 32.0 - 212 °F
IPC TM-650 2.4.24
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 0.000 - 100 °C
44.4 µin/in-°F

@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.320 W/m-K

@Temperature 100 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1225
Flammability, UL94 V-0
V-0
Vertical Burn
Electrical Properties Metric English Comments
Volume Resistivity 1.10e+15 ohm-cm
1.10e+15 ohm-cm
C96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 4.50e+13 ohm
4.50e+13 ohm
C96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
C23/50; IPC TM-650 2.5.5.3
2.6

@Frequency 1.00e+10 Hz
2.6

@Frequency 1.00e+10 Hz
C23/50; IPC TM-650 2.5.5.5
2.6

@Frequency 2.00e+8 Hz
2.6

@Frequency 2.00e+8 Hz
C23/50; IPC TM-650 2.5.5.6
Dielectric Breakdown >= 45000 V
>= 45000 V
D48/50; ASTM D149
Dissipation Factor 0.00135

@Frequency 1.00e+6 Hz
0.00135

@Frequency 1.00e+6 Hz
Loss Tangent, C23/50; IPC TM-650 2.5.5.3
0.0017

@Frequency 1.00e+10 Hz
0.0017

@Frequency 1.00e+10 Hz
Loss Tangent, C23/50; IPC TM-650 2.5.5.6
Arc Resistance >= 180 sec
>= 180 sec
D48/50; ASTM D495
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -80
IPC TM-650 2.5.5.5 (-10 - 140°C)