H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
Particle Size 22 - 26 µm
22 - 26 µm
10%
38 - 46 µm
38 - 46 µm
50%
65 - 75 µm
65 - 75 µm
90%
125 µm
125 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 9.0 - 11 %
9.0 - 11 %
Iron, Fe <= 0.50 %
<= 0.50 %
Nickel, Ni 18 - 22 %
18 - 22 %
Oxygen, O <= 0.60 %
<= 0.60 %