Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 25CAR+5CER PTFE; Petroleum Coke and Ceramic Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke + 5 wt.% Ceramic. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectr.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Density | 2.08 g/cc | 0.0750 lb/in³ | Yield Density |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Density | 2.08 g/cc | 0.0752 lb/in³ | |
Saint-Gobain Chemfab® 14 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: .. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific) LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
Sawbones Second-Generation Simulated Cortical Bone E-glass / Epoxy CompositeSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous .. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ISO 1183 |
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ISO 1183 |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ISO 1183 |
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
Zircar Refractory Composites RS-DD Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | after drying @ 100°C |
Zircar Refractory Composites RS-DM Refractory Sheet TYPE RS-DM Sheet is a moldable form of Type RS-D with a higher density than obtainable from Refractory Sheet Type RS-DA. Type RS-DM is ideally suited for fabricating complex shapes from a flat sheet.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
Zircar Refractory Composites RS-DR Refractory Sheet TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
Zircar Refractory Composites RS-202 Refractory Sheet ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Density | 2.08 g/cc | 0.0752 lb/in³ | |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Density | 2.08 g/cc | 0.0752 lb/in³ | |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | |
BASF Heligoen® Green L 8605 Color Additive Description: Bluish phthalocyanine greenChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing.. |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 63001 Anti-split HPP. 85% CaCO3 Filled.Price Competitive.Information provided by Multibase |
|||
Density | 2.08 g/cc | 0.0751 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 35CAR B PTFE; Carbon Filled
(discontinued **) Data provided by the manufacturer.35 wt.% Electrog. Carbon Filler. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope.. |