Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific) LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50004 Anti-blocking Masterbatch LDPE. 70% CaCO3 FilledInformation provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 50004 Anti-split HPP. 70% CaCO3 Filled.Thermal Resistance.Information provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
SGL Carbon Group Ridurid® EK 60 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Density | 1.74 g/cc | 0.0628 lb/in³ | |
Unifrax Fiberfrax® QF-180™ Coating Cement Fiberfrax QF-180™, QF-180™ Blue, and QF-150™ coating cements provide a range of consistencies for brush, spray, and trowel-on application. These coatings have 1260°C (2300°F) temperature grade.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive) Carbon-powder-filled, thermally stable, conductive material with consistent resistivities |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Devcon Carbide Putty Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fixture Elements, HousingsProcessing: Injection Molding (Melt Temperature:.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |