Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.59 g/cc | 0.0574 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Density | 1.59 - 1.86 g/cc | 0.0574 - 0.0672 lb/in³ | Average value: 1.75 g/cc Grade Count:15 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued * The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPET® KP133G30 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Density | 1.59 g/cc @Temperature 40.0 °C |
0.0574 lb/in³ @Temperature 104 °F |
|
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF1750-BK1 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC630 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | dry; ISO 1183 |
DSM Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 500 GB6 POM 30% glass beads filled low viscosity grade with very high stiffness and hardness with lowered shrinkage combined with easy molding of complicated shapesInformation provided by Zakłady Azotowe w .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 2527 POM Copolymer, 25% glass fiber reinforced POM-GF25Information provided by BARLOG plastics GmbH. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-251 Gray Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air.. |
|||
Density | 1.59 g/cc @Temperature 23.0 °C |
0.0574 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 2651MM/11 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 51030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |