Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D201 GF20 PBT, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.46 - 1.58 g/cc | 0.0527 - 0.0571 lb/in³ | Average value: 1.50 g/cc Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF008XXZ is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, Conditioned Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183-87 |
Wellman EcoLon® MRGF1518-BK3 38% Mineral/Glass Reinforced Post Consumer Compound Nylon 66 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 73 Flexible PVC, Sheathing General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/2 Flexible PVC, Sheathing General purposes |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry