Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East) LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Density | 1.44 - 1.48 g/cc | 0.0520 - 0.0535 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | Laminate Density |
Hardwire 3x2-4-12 Low Density Composite The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam.. |
|||
Density | 1.44 - 1.56 g/cc | 0.0520 - 0.0564 lb/in³ | Apparent |
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Teijin Panlite® GN-3430R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 30% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Polyplastics Duracon® TR-5 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | Cured |
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.44 - 1.48 g/cc | 0.0520 - 0.0535 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 65/C Flexible PVC, Injection Molding, Lead Free Mats |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.Data provided by the manufacturer |
|||
Density | 1.44 - 1.53 g/cc | 0.0520 - 0.0553 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Abatron AboCast 8708-6 One-Component Structural/Dielectric Epoxy AboCast 8708-6 is a highly filled, class H (180°C) structural, castable adhesive compound for SLOW high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; Emb.. |
|||
Density | 1.44 g/cc | 0.0519 lb/in³ | |
Abatron AboCast 8708-9 One-Component Structural/Dielectric Epoxy AboCast 8708-9 is a highly filled, class H (180°C) structural, castable adhesive compound for FASTER high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating; E.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific) LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Plenco 7697 Phenolic, Granular, Compression Molded PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |