Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.23 - 1.62 g/cc | 0.0444 - 0.0585 lb/in³ | Average value: 1.34 g/cc Grade Count:5 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | D Curative |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 CM16 HS BK 16% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 16% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East) LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D3165 |
Vicone High Performance Rubber VicoSil™ C240Q-RD High Performance Silicone Rubber Information provided by Vicone |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Covestro Desmopan® 359 Thermoplastic Polyurethane Desmopan 359 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23 Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L1 Wollastonite Reinforced |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Adell AR-13 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Adell AR-33 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
BASF Lupranate® M20FB Isocyanate Description: Lupranate® M20FB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20FB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH TS5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
BASF Lupranate® M20 Isocyanate Description: Lupranate® M20 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate M20 Isocyanate can be used for the production of rigid insulation foams by molding, sp.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
DuPont Performance Polymers Neoprene AD-5 Polychloroprene Rubber
(discontinued **) Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than neoprene AC during storage.Processing and .. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |