Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Plaskolite Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CP - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East) PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific) LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D1505 |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 2781 |
Lubrizol Advanced Materials PEARLBOND® 520 Linear Thermoplastic Polyurethane Pearlbond™ 520 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Chem Polymer Chemlon 182 Nylon 66, Flame Retarded A non-halogenated, unfilled nylon 66 used in electrical applications where improved flame retardancy is required. The material has excellent moldability, good snap-fit properties and is available i.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | Arlon SQA-TMS-024 |
Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 2781 |
Lubrizol Advanced Materials Pearlstick® 45-40/19 Polycaprolactone based TPU Pearlstick 45-40/19 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility: P.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 2781 |
Lubrizol Advanced Materials Pearlstick® 45-50/18 Polycaprolactone based TPU Pearlstick 45-50/18 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium-low thermoplasticity level. S.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Multibase Multi-Flam™ 0107 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingInformation provided by Multibase |