Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Plaskolite Duraplex® 70% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D-792 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D-792 |
Plaskolite Optix® CA - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **) Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | Yield Density |
Honeywell Capran® NyLid™ WMB 175 Nylon Lidding Film
(discontinued **) Description: Capran® NyLid™ WMB 175 is a 1.75 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 175 is suitable for die cutting, readily accept.. |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | Yield Density |
Honeywell Capran® Emblem™ 1200Matte Matte Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200Matte is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats,.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | |
Lord Adhesives 305 General Purpose, Medium Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Lucite International Colacryl ® LS200 Specialty Acrylic Resin Colacryl® LS200 is a medium-high molecular weight methyl methacrylate polymer. It is used mainly in coating applications where abrasion resistance and resistance to plasticiser migration are impo.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183-A |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9550 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PC/ABS FR 6206 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183-87 |
Wellman Wellamid® NY1599-GY Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183-87 |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Density | 1.16 - 1.18 g/cc | 0.0419 - 0.0426 lb/in³ | FTTC 2419 |
Formosa Plastics 35% Hydrochloric Acid Information provided by Formosa Plastics Corporation, USA |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Eurostar Staramide A40 PA66, Extrusion Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 62/T Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 55/A Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 58/1AT Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber transparent |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPC 30 PPC - 30% Calcium Carbonate Reinforced Polypropylene Copolymer 30% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Loctite® Gasket Eliminator® 510 Flange Sealant Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre.. |