Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH GF15020 PD1 NBR PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance Information Provided by LG Chem |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Density | 1.05 g/cc @Temperature 23.0 °C |
0.0379 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Inno-Comp INNOPOL® CS 1-2820 20% Glass-Fibre-Filled Polypropylene Homopolymer INNOPOL® CS 1-2820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-2820 is recommended for producing in.. |
|||
Density | 1.05 g/cc @Temperature 23.0 °C |
0.0379 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | Dry As Molded |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792B |
LyondellBasell Astryn 75F4-2 Polypropylene Copolymer, 20% Talc Key Features: conventional melt flow, medium high modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aestheticsApplications: small appli.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 (Asia Pacific) LNP* Lubriloy* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Tipco Tipcolene® DR 8201 - 20% Talc/Mineral Reinforced, Impact Modified, Polypropylene Copolymer 20% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Loctite® 222 Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Entec Hypro™ PPC-CC20 Natural Copolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM Epilac ABS-BLACK Acrylonitrile Butadiene Styrene |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Density | 1.05 g/cc | 0.0381 lb/in³ | |
Abatron AboGlass-1 Epoxy Decoupage Resin AboGlass-1 is a combination of a clear resin compound and a clear hardener. It is a virtually colorless, clear liquid, 2-part, epoxy system for casting layers up to 2 or more inches, and for embedme.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | Typical value for ABS |
Ashley Polymers Ashlene® ABS 220 High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Solvay RHODOCLEAN® ASP Surfactant Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Applications: Surfactant for metal working app.. |
|||
Density | 1.05 - 1.77 g/cc | 0.0379 - 0.0639 lb/in³ | Average value: 1.49 g/cc Grade Count:58 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |