| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
|
|||
| Density | 1.38 - 1.77 g/cc | 0.0499 - 0.0639 lb/in³ | Average value: 1.45 g/cc Grade Count:7 |
|
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
|
|||
| Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanical..
|
|||
| Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically ..
|
|||
| Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | Stand relative density |
|
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder
Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist..
|
|||
| Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D1505 |
|
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)
Hylar® 301F is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.Features: High Viscosity; HomopolymerUses: Coating ApplicationsAdditiona..
|
|||
| Density | 1.33 - 1.77 g/cc | 0.0480 - 0.0639 lb/in³ | Average value: 1.56 g/cc Grade Count:24 |
|
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
|
|||
| Density | 1.05 - 1.77 g/cc | 0.0379 - 0.0639 lb/in³ | Average value: 1.49 g/cc Grade Count:58 |
|
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..
|
|||