Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Pasargad Polymer Peyvand Pasalac 3P-H6000B ABS Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH K20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM Data |
Americas Styrenics Styron® 685P Polystyrene
(discontinued **) STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6111 Resin Supported Emulsion Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Global ABS-405 FR High Impact, Flame Retardant ABS Information provided by Global Polymers Corporation. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Iran Petrochemical (PCC) GPPS 1160 Polystyrene GPPS 1160 is a high heat resistance, high molecular weight crystalline polystyrene used in the extrusion industry. It is most suitable for production of oriented polystyrene. It is particularly use.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Momentive Performance Materials RTV5813 Black Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Shuman 710 Utility Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Styrolution PS 153A GPPS Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM Data |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene Saxalac 835U is an antistatic, easy flowing light stabilized ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical prop.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
American Polymers API 500 Polystyrene API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Entec Hypro™ PPC-GF20 Natural Impact Polypropylene, 20% Glass Reinforced Information provided by Entec |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183/A |
Addiplast Addilene J 522 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
A.D. Compound Adene NTFA Homopolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Ineos Nova 5120 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Solvay RHODAPEX® AB 20 Surfactant Description: APE free ether sulfate surfactant for emulsion polymerizationIdentification: AMMONIUM SALT OF SULPHATED ALCOHOL ETHOXYLATE.CAS: 67762 – 19 – 0Solubility: Soluble in water and most pol.. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792-91 |
Multibase Multi-ABS 3075 High Impact Data provided by Multibase. |
|||
Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
Borealis Daplen™ EF209AE Polypropylene TPO Compound Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |