Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mallard Creek Polymers Rovene® 6111 Resin Supported Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mallard Creek Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Rovene® 6111 Resin Supported Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film forming component in overprint varnish formulations or as the sole vehicle for inks and overprint varnishes providing good gloss. The emulsion can also be used as the non-skid component in formulations. Because of the low glass transition temperature, Rovene® 6104 has good adhesion to treated flexible films. Inks and overprint varnishes formulated with Rovene® 6104 can be formulated with graphic arts industry standard products and additives. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6111 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0377 lb/in³
Solids Content 47 - 50 %
47 - 50 %
pH 8.1 - 8.8
8.1 - 8.8
Brookfield Viscosity <= 1200 cP
<= 1200 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 104 °C
219 °F
Chemical Properties Metric English Comments
Total Acid Number 60
60
[mgKOH/g]