Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Petromont 4100 High Density Polyethylene Resin Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe
appl.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
PolyOne Syncure™ S1016A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1016A / 5 phr S1.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E904 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsInformation provided by Formosa Plastics Corporation, USA. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L4903 High Density Polyethylene ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5008 High Density Polyethylene ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with a.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LT570401 High Density Polyethylene ApplicationsPETROTHENE LT 5704-01 resin exhibits good stiffness and environment stress crack resistance. Typical applications are bleach and household chemical bottles.Regulatory StatusLT 5704-01 m.. |
|||
Density | 0.949 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GP 9452 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | |
JPJ Technologies 2300XM HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L4907 High Density Polyethylene ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5040TC High Density Polyethylene ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 4602 FA HDPE Film Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official dis.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Borealis Borstar® ME3446 Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black MD Pipe for Natural Gas Borstar 3446 is a bimodal, cadmium free, medium density polyethylene compound designed for coextrusion of yellow identifying stripes. It is fully stabilized against thermal degradation and the die .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total 49080 UV HDPE blow molding FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total MS 201 B N HDPE blow molding FINATHENE® MS 201 B N is a high density polyethylene produced by a low pressure slurry polymerization process. FINATHENE® MS 201 B N has been developed for the blow molding of Plastic Fuel Tanks a.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HB4903 Blow Molding HDPE Hexene CopolymerApplications: High performance blow molding applications, fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
Dow UNIPOL™ DGDA-5110 Polyolefin DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924F Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Film Applications Formolene® E924F is a “low gel” high molecular weight grade of HDPE designed for high dart impact strength and.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |