Material Notes:
FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the production of containers with a high impact strength, an excellent stress-crack resistance and a low creep under load. FINATHENE® 49080 UV is specially recommended for the blow-molding of Heating Oil Tank and large containers (IBC) dedicated to the transportation of dangerous goods (UN-regulations). Applications: shipping containers, industrial chemical tanks, intermediate bulk containers, agricultural chemical tanks. Blow Molding Stock Temperature 370 – 440 ºFInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
100% ant.; ASTM D1693-70
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133 cond. 7
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ISO 527
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 105 kJ/m²
50.0 ft-lb/in²
Notched, -30°C; ISO 8256
230 kJ/m²
109 ft-lb/in²
Notched, 23°C; ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ISO 306
Descriptive Properties Value Comments
Food Approval This material complies with the main regulations concerning non-toxicity of plastics materials in contact with food stuffs.