Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Reliance Industries Relene S42005 Polyethylene
Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended ..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil Method
ExxonMobil LL 3402.48 Cast Film Resin  (discontinued **)
LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the ..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Chevron Phillips mPact™ D449 HDPE Blown Film Resin  (discontinued **)
Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw..
Density 0.942 g/cc
0.0340 lb/in³
Base Density
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled  (discontinued **)
Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi..
Density 0.942 - 0.949 g/cc
0.0340 - 0.0343 lb/in³
Average value: 0.946 g/cc Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
Ineos K38-20-160 Polyethylene Copolymer
K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D 4883
Ineos K38-20X2091 HDPE
K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m..
Density 0.942 - 0.946 g/cc
0.0340 - 0.0342 lb/in³
DIN 53479
Iran Petrochemical (PCC) Arak EX3 HDPE
Information provided by Iran Petrochemical Commercial Co.
Density 0.942 g/cc
0.0340 lb/in³
ASTM D792
LyondellBasell Hostacomâ„¢ 6551 Polypropylene Homopolymer
Description: Hostacomâ„¢ 6551 conventional melt flow, 1,300 MPa flexural modulus, precolored polypropylene homopolymer has a good combination of strength, stiffness, impact and heat resistance. I..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D792
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes...
Density 0.942 g/cc
0.0340 lb/in³
ISO 1183
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes
BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr..
Density 0.942 g/cc
0.0340 lb/in³
Base; ASTM D792
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important ..
Density 0.942 g/cc
0.0340 lb/in³
ISO 1183
Unipetrol PE HD LITEN® BB 10 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Density 0.942 g/cc
0.0340 lb/in³
ISO 1183
Unipetrol PE HD LITEN® FB 10 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Westlake EMAC® Plus SP1307 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1307 is a 20% EMA copolymer designed for extrusion coating, laminations, and blending where EMA properties are needed, but higher temperature resistance is required. SP1307 is..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D1505
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
Westlake Tymax™ GA7001 Anhydride Modified Acrylate Copolymer (Developmental)
Westlake GA7001 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications. W..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin ..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin
Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil Method
ExxonMobil Escorene® LD 721.IK Film Resin
Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,..
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Ap..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
ExxonMobil HDP8660.29 Rotational Molding Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products
Density 0.942 g/cc
0.0340 lb/in³
ASTM D4883
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products
Density 0.942 g/cc
0.0340 lb/in³
ASTM D792
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin  (discontinued **)
Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals.
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil Method
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin  (discontinued **)
ESCOR AT 310 provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier ..
Density 0.942 g/cc
0.0340 lb/in³
Base Resin; ASTM D792
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by..
Copyright © lookpolymers.com All Rights Reserved