Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Copolymer Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.942 - 0.949 g/cc
0.0340 - 0.0343 lb/in³
Average value: 0.946 g/cc Grade Count:4
Melt Flow 0.250 - 0.400 g/10 min
0.250 - 0.400 g/10 min
Average value: 0.313 g/10 min Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Shore D 59.0 - 70.0
59.0 - 70.0
Average value: 63.0 Grade Count:3
Film Tensile Strength at Yield, MD 21.0 - 22.0 MPa
3050 - 3190 psi
Average value: 21.3 MPa Grade Count:3
Film Tensile Strength at Yield, TD 22.0 - 24.0 MPa
3190 - 3480 psi
Average value: 23.0 MPa Grade Count:3
Film Elongation at Break, MD 430 - 600 %
430 - 600 %
Average value: 520 % Grade Count:3
Film Elongation at Break, TD 850 - 900 %
850 - 900 %
Average value: 881 % Grade Count:3
Secant Modulus, MD 0.510 - 0.638 GPa
74.0 - 92.5 ksi
Average value: 0.579 GPa Grade Count:3
Secant Modulus, TD 0.680 - 0.769 GPa
98.6 - 112 ksi
Average value: 0.713 GPa Grade Count:3
Elmendorf Tear Strength, MD 0.500 - 1.00 g/micron
12.7 - 25.4 g/mil
Average value: 0.700 g/micron Grade Count:3
Elmendorf Tear Strength, TD 18.7 - 26.0 g/micron
475 - 660 g/mil
Average value: 22.6 g/micron Grade Count:3
Dart Drop 0.600 - 2.70 g/micron
15.2 - 68.6 g/mil
Average value: 1.54 g/micron Grade Count:3
Film Tensile Strength at Break, MD 35.0 - 54.0 MPa
5080 - 7830 psi
Average value: 43.0 MPa Grade Count:3
Film Tensile Strength at Break, TD 33.0 - 39.0 MPa
4790 - 5660 psi
Average value: 36.7 MPa Grade Count:3