Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene re.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Reliance Industries Reclair R35042 Polyethylene Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-708 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1475 |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 110-1332 LMDPE Rotational Molding Resin Description: ICORENE 110-1332 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1652 LMDPE Rotational Molding Resin Description: ICORENE 115-1652 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 190-1332 LMDPE Rotational Molding Resin Description: ICORENE 190-1332 is a compounded linear density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Density | 0.935 g/cc @Temperature 260 °C |
0.0338 lb/in³ @Temperature 500 °F |
Melt |
Covestro Bayblend® T45 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ExxonMobil method |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2038 Linear Low Density Polyethylene Linear Low Density PolyethyleneInformation provided by Dow |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM-D1505 |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 50-3 |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 7804-3 |
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 7804-4 |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | |
Beijing Evergrow Resources UHMW PE Powder Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.Features:Very high abrasion resistanceVery high impact streng.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |