Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.920 g/cc | 0.0332 lb/in³ | |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
PolyOne Syncure™ S1017B Polyethylene, Crosslinked (XLPE) Available as Catalyst Masterbatch component for PolyOne Syncure System.Oven Aging values are >75, and were measured on a 98.5 phr S1025A / 1.5 phr S1017B Syncure System. Torque is >1500. Pellet appe.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock, Process Aid Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D4883 |
Eastman Voridian D4053-A Polyethylene
(discontinued **) Voridian polyethylene D4053-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on aut.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
Entec Hypel® PELD12/.920 LDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 214 Low Density Polyethylene
(discontinued **) IPETHENE® 214 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. APPLICATIONS IPETHENE® 214 is main.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture fil.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183 |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183 |
Borealis FT3200 Low Density Polyethylene FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ra.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM-D792 |
CTC X-PRO CTC PP1050 Polypropylene Homopolymer X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Density | 0.920 g/cc @Temperature 15.6 °C |
0.0332 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Extra Hecta Super Mineral Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | |
Dow Elite® 5100 Linear Low Density Polyethylene 5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 322 Low Density Polyethylene IPETHENE® 322 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between .. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. .. |
|||
Density | 0.920 g/cc @Temperature 40.0 °C |
0.0332 lb/in³ @Temperature 104 °F |
|
BASF Hexamethylenediamine 70% Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | |
Von Roll Isola IMI Irrathene® 201 Irradiated Polyethylene Film Data provided by Von Roll Isola USA.Produced by electron bombardment of specially formulated polyethylene film used in a wide variety of electrical applications. Irrathene film is nonmelting and hi.. |