Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Zylog Plastalloys
Trade Name Neoplast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D 2240
93

@Time 605000 sec
93

@Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 16.7 MPa
2420 psi
500 mm/min; ASTM D 412
18.3 MPa

@Time 605000 sec
2660 psi

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 600 %
600 %
500 mm/min; ASTM D 412
528 %

@Time 605000 sec
528 %

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.0108 GPa
1.56 ksi
500 mm/min; ASTM D 412
Tear Strength 49.0 kN/m
280 pli
500 mm/min; ASTM D 624
Compression Set 48 %

@Temperature 23.0 °C,
Time 79200 sec
48 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Continuous; SAE J 2236
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D 746