Mechanical Properties Metric English Comments
Tear Strength 49.0 kN/m
280 pli
ASTM D624
Multibase Multi-Flex® TPE A 8502 CLASSY GREY
Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 15%. Multi-Flex TPE contains Krato..
Tear Strength 49.0 kN/m
280 pli
Die C, 510 mm/min; ASTM D624
PolyOne Elastamax™ XL-2175 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tear Strength 49.0 kN/m
280 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tear Strength 49.0 kN/m
280 pli
49 kN/m at 23°C. Value at 100°C is 23 kN/m. TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
Tear Strength 49.0 kN/m
280 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 49.0 kN/m
280 pli
Die C, 510 mm/min; ASTM D624
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tear Strength 49.0 kN/m
280 pli
B-type, Vulcanized
KKPC KOSYN 1502G Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 49.0 kN/m
280 pli
B-type, Vulcanized
KKPC KOSYN 1502LL Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 49.0 kN/m
280 pli
B-type, Vulcanized
KKPC KOSYN 1502NF Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 49.0 kN/m
280 pli
B-type, Vulcanized
KKPC KOSYN 1507L Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 49.0 kN/m
280 pli
B-type, Vulcanized
KKPC KOSYN 1507 Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tear Strength 49.0 kN/m
280 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 850A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 49.0 kN/m
280 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 49.0 kN/m
280 pli
ASTM D624
SK Chemicals SKYTHANE® UB410 Powder Coating
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tear Strength 49.0 kN/m
280 pli
ASTM D624
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 49.0 kN/m
280 pli
500 mm/min; ASTM D 624
Zylog Neoplast® 180 C Thermoplastic Vulcanizate
Neoplast 180 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV S..
Tear Strength 49.0 kN/m
280 pli
500 mm/min; ASTM D 624
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate
Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Tear Strength 49.0 kN/m
280 pli
ISO 34B
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av..
Tear Strength 49.0 kN/m
280 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler