Zeon Chemicals Zetpol® 2010 Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 2010 Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zetpol 2010 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.For O-rings, gaskets, seals, or oil field components requiring the best balance of heat and compression set. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number 8.0 - 14
8.0 - 14
mg/100mg; ZCI-T-004
Mooney Viscosity 78 - 92

@Temperature 100 °C
78 - 92

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 66 - 74
66 - 74
ZCI-T-009
Tensile Strength at Break 25.19 - 31.19 MPa
3654 - 4524 psi
ZCI-T-008
Elongation at Break 350 - 510 %
350 - 510 %
ZCI-T-008
300% Modulus 0.01440 - 0.02239 GPa
2.088 - 3.248 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 96
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 0.5