Tensile Strength at Break 25.19 - 31.19 MPa
3654 - 4524 psi
ZCI-T-008
Zeon Chemicals Zetpol® 2010 Hydrogenated Nitrile Elastomomer
Zetpol 2010 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance o..