Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Zetpol® 2000L Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 2000L Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zeptol 2000L is a low-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.Low Mooney version of Zetpol 2000. Excellent for transfer or injection molding. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number <= 7.0
<= 7.0
mg/100mg; ZCI-T-004
Mooney Viscosity 58 - 72

@Temperature 100 °C
58 - 72

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 71
65 - 71
ZCI-T-009
Tensile Strength at Break 22.59 - 28.39 MPa
3277 - 4118 psi
ZCI-T-008
Elongation at Break 450 - 550 %
450 - 550 %
ZCI-T-008
300% Modulus 0.01080 - 0.01670 GPa
1.566 - 2.422 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD >99.5
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 0.5
Users viewing this material also viewed the following: