Polymer Property : Tensile Strength at Break = 3277 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.59 - 28.39 MPa
3277 - 4118 psi
ZCI-T-008
Zeon Chemicals Zetpol® 2000L Hydrogenated Nitrile Elastomomer
Zeptol 2000L is a low-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good chemical resistance to aggressive flui..
Tensile Strength at Break 22.59 - 28.39 MPa
3277 - 4118 psi
ZCI-T-008
Zeon Chemicals Zetpol® 2000LL Hydrogenated Nitrile Elastomomer
Zeptol 2000LL is the lowest Mooney version of a highly saturatred copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good chemcial resistance to aggressi..