EMS-Griltech Grilon® BA 3100 White Nylon 66/Nylon 6 Bi-Component Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 66 , Nylon 66 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® BA 3100 White Nylon 66/Nylon 6 Bi-Component Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON BA 3100 is the new core / sheath bi-component fiber based on PA 66/PA 6 with a sheath melting range from 215 - 225 °C. The fine count bi-component fiber guarantees an even distribution of the adhesive in the fiber bond. It is preferably used for thermofusing of nonwovens and yarns. Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 3.30 - 6.70 dtex
2.97 - 6.03 denier
Thermal Properties Metric English Comments
Melting Point 215 - 225 °C
419 - 437 °F
Sheath
Descriptive Properties Value Comments
Color Raw White
Luster Semidull
Staple Length 51-60 mm