Zeon Chemicals Nipol® DN631 Carboxylated Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® DN631 Carboxylated Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases.Exhibits good oil resistance and high tensile strength, and is used in belt, seal, and roll applications.
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
Mooney Viscosity 48 - 63

@Temperature 100 °C
48 - 63

@Temperature 212 °F
(1+4)
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 33
Hot/Cold C