Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals HyTemp® SC-75 Polyacrylate Curative

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® SC-75 Polyacrylate Curative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp SC-75 is a 75% active dispersion of a proprietary cure system. The dispersion functions as a cure package in HyTemp 4050 series elastomers. This provides fast property development; excellent shelf stability and good scorch resistance. The dispersion is in the form of green pellets dusted with clay and free from foreign materials.Fast cure package for HyTemp 4050 and 4060 series (75% active)
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
Component Elements Properties Metric English Comments
Nitrogen, N 3.4 - 4.8 %
3.4 - 4.8 %
Copyright © lookpolymers.com All Rights Reserved