Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM 792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Melt Flow 1.01 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.01 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.4 MPa
7450 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Flexural Modulus 3.20 GPa
464 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
Unannealed; ASTM D648